NORMSERVIS s.r.o.

ASTM A691/A691M-19

Standard Specification for Carbon and Alloy Steel Pipe, Electric-Fusion-Welded for High-Pressure Service at High Temperatures

STANDARD published on 1.11.2019

English -
PDF - Immediate download (63.00 USD)

English -
PDF + redline - Immediate (75.60 USD)

English -
Print design (63.00 USD)

English -
Print + redline (75.60 USD)


Why Redline?

A PDF redline is a quick and easy way to compare all of the changes between the current, active standard and the previous version.

With a redline you'll immediately see:

Save Time and Trouble!

With a Redline you no longer have to spend time trying to determine what has changed in the new standard! Redlines save you time and ensure you see what the changes are to the standard.

Price

When you select the "Active + Redline" option you get both documents! Best of all, the cost of an Active + Redline is only slightly more than buying the Active Standard by itself.

View Sample Redline

The information about the standard:

Designation standards: ASTM A691/A691M-19
Publication date standards: 1.11.2019
The number of pages: 7
Approximate weight : 21 g (0.05 lbs)
Country: American technical standard
Category: Technical standards ASTM

Annotation of standard text ASTM A691/A691M-19 :

This specification covers carbon and alloy steel pipe, electric-fusion-welded with filler metal added, fabricated from pressure-vessel-quality plate of several analyses and strength levels and suitable for high-pressure service at high temperatures. Heat treatment may or may not be required to attain the desired mechanical properties. The pipes are classified according to steel grades and are designated in classes according to the type of heat treatment performed in the pipe manufacture, whether the weld is radiographically examined, and whether the pipe has been pressure tested. The steel welds shall be made either manually or automatically by an electric process involving the deposition of filler metal. The welded joints shall have positive reinforcement at the center of each side of the weld. The contour of this reinforcement shall be smooth, and the deposited metal shall be fused smoothly and uniformly into the plate surface. The joints shall undergo tension, bend and pressure tests. Unacceptable surface imperfections shall be removed by grinding or machining. The depression after grinding or machining shall be blended uniformly into the surrounding surface. Repair of weld and base metal defects shall be done by welding.


Keywords:
ICS Number Code 23.040.10 (Iron and steel pipes)