NORMSERVIS s.r.o.

ASTM A384/A384M-24

Standard Practice for Safeguarding Against Warpage and Distortion During Hot-Dip Galvanizing of Steel Assemblies

STANDARD published on 1.4.2024

English -
PDF - Immediate download (55.00 USD)

English -
PDF + redline - Immediate (66.00 USD)

English -
Print design (55.00 USD)

English -
Print + redline (66.00 USD)


Why Redline?

A PDF redline is a quick and easy way to compare all of the changes between the current, active standard and the previous version.

With a redline you'll immediately see:

Save Time and Trouble!

With a Redline you no longer have to spend time trying to determine what has changed in the new standard! Redlines save you time and ensure you see what the changes are to the standard.

Price

When you select the "Active + Redline" option you get both documents! Best of all, the cost of an Active + Redline is only slightly more than buying the Active Standard by itself.

View Sample Redline

The information about the standard:

Designation standards: ASTM A384/A384M-24
Publication date standards: 1.4.2024
The number of pages: 3
Approximate weight : 9 g (0.02 lbs)
Country: American technical standard
Category: Technical standards ASTM

Annotation of standard text ASTM A384/A384M-24 :

This specification deals with safeguarding against warpage and distortion during hot-dip galvanizing of steel assemblies. Common distorted and warped members of assemblies are sheets or plates assembled by welding or riveting. The following can cause warpage and distortion: use of nonsymmetrical sections such as channels; use of checkered plate; not properly vented overlapping joint for two pieces of steel; and too large assembly for a particular galvanizing kettle. Suggested corrections for panel fabrication are detailed.


Keywords:
coatings-zinc, galvanized coatings, steel products-metallic coated, zinc coatings-steel products,, ICS Number Code 25.220.20 (Surface treatment)