NORMSERVIS s.r.o.

ASTM B247M-20

Standard Specification for Aluminum and Aluminum-Alloy Die Forgings, Hand Forgings, and Rolled Ring Forgings (Metric)

STANDARD published on 1.5.2020

English -
PDF - Immediate download (69.00 USD)

English -
PDF + redline - Immediate (82.80 USD)

English -
Print design (69.00 USD)

English -
Print + redline (82.80 USD)


Why Redline?

A PDF redline is a quick and easy way to compare all of the changes between the current, active standard and the previous version.

With a redline you'll immediately see:

Save Time and Trouble!

With a Redline you no longer have to spend time trying to determine what has changed in the new standard! Redlines save you time and ensure you see what the changes are to the standard.

Price

When you select the "Active + Redline" option you get both documents! Best of all, the cost of an Active + Redline is only slightly more than buying the Active Standard by itself.

View Sample Redline

The information about the standard:

Designation standards: ASTM B247M-20
Publication date standards: 1.5.2020
The number of pages: 14
Approximate weight : 42 g (0.09 lbs)
Country: American technical standard
Category: Technical standards ASTM

Annotation of standard text ASTM B247M-20 :

This specification covers aluminum and aluminum-alloy die forgings, hand forgings, and rolled ring forgings and includes the following UNS alloy designations: A91100, A92014, A92018, A92025, A92219, A92618, A93003, A94032, A95083, A96061, A96066, A96151, A97049, A97050, A97075, A97076, and A97175. Tempers covered by this specification includes: H112, T4, T6, T61, T73, T74, T7352, T7452, T7454, T652, T852, and H111 as well as F and 01 types. The forgings may be manufactured by pressing, hammering, or rolling, at the option of the producer. Requirements for quality assurance, chemical analysis, tension and hardness tests, heat treatment, heat-treat response, and stress corrosion resistance and stress-corrosion cracking test are detailed. The forgings shall conform to the chemical composition requirements prescribed for aluminum, silicon, iron, copper, manganese, magnesium, chromium, nickel, zinc, zirconium, and titanium. Forgings having the specified thickness shall meet the requirements specified for the mechanical properties such as tensile strength, yield strength, elongation, and Brinell hardness.


Keywords:
aluminum alloy, die forgings, hand forgings, rolled ring forgings,, ICS Number Code 77.150.10 (Aluminium products)