NORMSERVIS s.r.o.

SAE AMS5661G

Nickel-Iron Alloy, Corrosion and Heat-Resistant, Bars, Forgings, and Rings 42.5Ni - 12.5Cr - 5.8Mo - 2.9Ti - 0.015B - 35Fe Consumable Electrode or Vacuum Induction Melted Solution, Stabilization, and Precipitation Heat Treated

STANDARD published on 1.8.2018

English -
electronic design (pdf) (100.10 USD)

English -
Print design (100.10 USD)

The information about the standard:

Designation standards: SAE AMS5661G
Note: Historical
Publication date standards: 1.8.2018
Country: American technical standard
Category: Technical standards SAE