NICKEL ALLOY, CORROSION AND HEAT RESISTANT, BARS, FORGINGS, AND RINGS 52.5Ni - 19Cr - 3.0Mo - 5.1(Cb + Ta) - 0.90Ti - 0.5Al - 18Fe Consumable Electrode or Vacuum Induction Melted 1775 °F (968 °C) Solution Heat Treated, Precipitation Hardenable
STANDARD published on 1.1.1993
Designation standards: SAE AMS5662G
Note: Historical
Publication date standards: 1.1.1993
Country: American technical standard
Category: Technical standards SAE