Nickel Alloy, Corrosion and Heat-Resistant, Bars, Forgings, and Rings 57Ni - 19.5Cr - 13.5Co - 4.3Mo - 3.0Ti - 1.4Al - 0.05Zr - 0.006B Consumable Electrode Remelted or Vacuum Induction Melted 1825 to 1900 °F (996 to 1038 °C) Solution, Stabilization, and Precipitation Heat Treated
STANDARD published on 1.1.2015
Designation standards: SAE AMS5707M
Note: Historical
Publication date standards: 1.1.2015
Country: American technical standard
Category: Technical standards SAE