Cobalt-Nickel Alloy, Corrosion and Heat Resistant, Bars 19Cr - 36Co - 25Ni - 7.0Mo - 0.50Cb - 2.9Ti - 0.20Al - 9.0Fe Vacuum Induction Plus Vacuum Consumable Electrode Melted Solution Heat Treated for Work Strengthening
STANDARD published on 1.10.2000
Designation standards: SAE AMS5841D
Note: Historical
Publication date standards: 1.10.2000
Country: American technical standard
Category: Technical standards SAE