We need your consent to use the individual data so that you can see information about your interests, among other things. Click "OK" to give your consent.
Standard Test Method for dc Magnetic Properties of Materials Using Ring and Permeameter Procedures with dc Electronic Hysteresigraphs
STANDARD published on 1.5.2009
Designation standards: ASTM A773/A773M-01(2009)
Note: WITHDRAWN
Publication date standards: 1.5.2009
SKU: NS-4112
The number of pages: 10
Approximate weight : 30 g (0.07 lbs)
Country: American technical standard
Category: Technical standards ASTM
Keywords:
dc hysteresigraph, dc hysteresis, Epstein test, Hall probe, hysteresis loop, permeameter, ring-type specimen, Current measurement--direct-current, D-c magnetic properties, Direct-current permeability, Hysteresis effects, Permeameters (direct-current), Ring test procedures, ICS Number Code 29.030 (Magnetic materials)
Significance and Use | ||||||||||||||||
Hysteresigraph testing permits more rapid and efficient collection of dc hysteresis (B-H loop) data as compared to the point by point ballistic Test Methods A 341/A 341M and A 596/A 596M. The accuracy and precision of testing is comparable to the ballistic methods. Hysteresigraphs are particularly desirable for testing of semihard and hard magnetic materials where either the entire second quadrant (demagnetization curve) or entire hysteresis loop is of primary concern. Provided the test specimen is representative of the bulk sample or lot, this test method is well suited for design, specification acceptance, service evaluation and research and development. |
||||||||||||||||
1. Scope | ||||||||||||||||
1.1 This test method provides dc hysteresigraph procedures (B-H loop methods) for the determination of basic magnetic properties of materials in the form of ring, toroidal, link, double-lapped Epstein cores, or other standard shapes that may be cut, stamped, machined, or ground from cast, compacted, sintered, forged, or rolled materials. It includes tests for normal induction and hysteresis taken under conditions of continuous sweep magnetization. Rate of sweep may be varied, either manually or automatically at different portions of the curves during tracing. Total elapsed time for tracing a hysteresis loop is commonly 10 to 120 s per loop. 1.2 The values stated in either SI units or inch-pound units are to be regarded separately as standard. The values stated in each system may not be exact equivalents; therefore, each system shall be used independently of the other. Combining values from the two systems may result in non-conformance with the standard. 1.3 This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety and health practices and determine the applicability of regulatory limitations prior to use. |
||||||||||||||||
2. Referenced Documents | ||||||||||||||||
|
Do you want to be sure about the validity of used regulations?
We offer you a solution so that you could use valid and updated legislative regulations.
Would you like to get more information? Look at this page.
Latest update: 2025-07-04 (Number of items: 2 207 347)
© Copyright 2025 NORMSERVIS s.r.o.