We need your consent to use the individual data so that you can see information about your interests, among other things. Click "OK" to give your consent.
Standard Guide for Specifying Harmonized Standard Grade Compositions for Wrought Stainless Steels (Includes all amendments And changes 8/16/2017).
Automatically translated name:
Standard Guide for Specifying Harmonized Standard Grade Compositions for Wrought Stainless Steels
STANDARD published on 10.10.2001
Designation standards: ASTM A959-00a
Note: WITHDRAWN
Publication date standards: 10.10.2001
SKU: NS-5018
The number of pages: 7
Approximate weight : 21 g (0.05 lbs)
Country: American technical standard
Category: Technical standards ASTM
Keywords:
austenitic stainless steels, austenitic-ferritic or ferritic-austenitic stanless steels, duplex stainless steels, ferritic stainless steels, harmonized stainless steel compositions, martensitic stainless steels, precipitation hardening stainless steels, standard stainless steel grade compositions, ICS Number Code 77.140.20 (Steels of high quality)
| 1. Scope | ||||||||
|
1.1 This standard provides a guide to ASTM Subcommittees A01.06, A01.10, A01.17, A01.22, and A01.28 for specifying chemical composition limits of wrought stainless steels. It is intended that these recommended grade composition limits be suitable for adoption by other standardization bodies that prepare standards for stainless steel products. 1.2 Included in this guide are the recommendations for determining the number of significant figures for specifying chemical composition from Test Methods, Practices and Terminology A 751. 1.3 All stainless steel UNS numbers and the stainless steel grades in all standards overseen by the aforementioned ASTM subcommittees have been included, except those grades applicable to restricted special end uses and alloys containing less than 10.5 % minimum chromium. 1.4 Not addressed are minor composition modifications which a specific product subcommittee may find necessary to accommodate effects of normal processing or to enhance fabricability by the producer or user, or both. 1.5 Also not generally addressed (except when established by ASTM product subcommittees) is a complete rationalization of all limits, especially when such would conflict with long-standing practices and is not justified by special technical effect. 1.6 Excluded from this guide are cast material and welding filler metal. |
||||||||
| 2. Referenced Documents | ||||||||
|
Do you want to make sure you use only the valid technical standards?
We can offer you a solution which will provide you a monthly overview concerning the updating of standards which you use.
Would you like to know more? Look at this page.
Latest update: 2026-05-04 (Number of items: 2 275 493)
© Copyright 2026 NORMSERVIS s.r.o.