We need your consent to use the individual data so that you can see information about your interests, among other things. Click "OK" to give your consent.
Standard Specification for Nickel Rod and Bar (Includes all amendments And changes 10/8/2014).
Automatically translated name:
Standard Specification for Nickel Rod and Bar
STANDARD published on 1.10.2009
Designation standards: ASTM B160-05(2009)e1
Note: WITHDRAWN
Publication date standards: 1.10.2009
SKU: NS-5521
The number of pages: 6
Approximate weight : 18 g (0.04 lbs)
Country: American technical standard
Category: Technical standards ASTM
Keywords:
bar, rod, N02200, N02201, N02211, Nickel--specifications, Nickel alloy rod/bar/wire--specifications, UNS N02200 (commercially pure Ni alloy, Nickel 200), UNS N02201 (commercially pure Ni alloy, Nickel 201), ICS Number Code 2211, 77.150.40 (Nickel and chromium products)
1. Scope | ||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||
1.1 This specification covers nickel (UNS N02200)*, low carbon nickel (UNS N02201)*, and solution strengthened nickel (UNS N02211) in the form of hot-worked and cold-worked rod and bar in the conditions shown in Table 1. 1.2 The values stated in inch-pound units are to be regarded as standard. The values given in parentheses are mathematical conversions to SI units that are provided for information only and are not considered standard. 1.3 This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to become familiar with all hazards including those identified in the appropriate Material Safety Data Sheet (MSDS) for this product/material as provided by the manufacturer, to establish appropriate safety and health practices, and determine the applicability of regulatory limitations prior to use. TABLE 1 Mechanical Properties
A See 12.2. B Not applicable to diameters or cross sections under 3/32 in. (2.4 mm). C For hot-worked flats 5/16 in. (7.9 mm) and under in thickness the elongation shall be 25%, min. D Hardness B45 to B80, or equivalent. E Hardness B45 to B70 or equivalent. F Forging quality is furnished to chemical requirements and surface inspection only. No tensile properties are required. |
||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||
2. Referenced Documents | ||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||
|
Do you want to make sure you use only the valid technical standards?
We can offer you a solution which will provide you a monthly overview concerning the updating of standards which you use.