We need your consent to use the individual data so that you can see information about your interests, among other things. Click "OK" to give your consent.
Standard Test Method for Measurement of Internal Stress of Metallic Coatings by Split Strip Evaluation (Deposit Stress Analyzer Method)
STANDARD published on 1.11.2015
Designation standards: ASTM B975-15
Note: WITHDRAWN
Publication date standards: 1.11.2015
SKU: NS-623193
The number of pages: 8
Approximate weight : 24 g (0.05 lbs)
Country: American technical standard
Category: Technical standards ASTM
Keywords:
deposit stress analyzer method, helix, internal deposit stress, metallic coatings, modulus of elasticity, spiral contractometer method, test strip ,, ICS Number Code 25.220.40 (Metallic coatings)
| Significance and Use | ||||||||
|
5.1 Internal stress in applied coatings exhibits potential to cause a breakdown of resistance to corrosion and erosion as a result of the formation of fractures from micro-cracking and macro-cracking within the applied coating. This phenomenon can also cause blistering, peeling, reduction of fatigue strength, and loss. The resulting stress can be tensile in nature, causing the deposit to contract, or compressive in nature, causing the deposit to expand. 5.2 To maintain quality assurance by the bent strip method, it is necessary to monitor production processes for acceptable levels of internal deposit stress in applied coatings. Note that the highest value of the internal deposit stress as obtained on a stress-versus-coating-thickness curve is usually the truest value of the internal deposit stress. Most low values are false. Initial values tend to be lower than the actual value because of the effect of stock material edge burrs and the resistance of the stock material to bending. Excessive deposit thickness causes lower-than-true values since the coating overpowers and changes the initial modulus of elasticity of the test piece, which becomes more difficult to bend as the coating continues to build upon it. This phenomenon can be corrected considerably by use of a formula that compensates for modulus of elasticity differences between the deposit and the substrate materials, but it does remain a factor. See Eq 2. |
||||||||
| 1. Scope | ||||||||
|
1.1 This test method for determining the internal tensile or compressive stress in applied coatings is quantitative. It is applicable to metallic layers that are applied by the processes of electroplating or chemical deposition that exhibit internal tensile or compressive stress values from 500 to 145 000 psi (3.45 to 1000 MPa). 1.2 The values stated in inch-pound units are to be regarded as standard. The values given in parentheses are mathematical conversions to SI units that are provided for information only and are not considered standard. 1.3 This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety and health practices and determine the applicability of regulatory limitations prior to use. |
||||||||
| 2. Referenced Documents | ||||||||
|
Do you want to be sure about the validity of used regulations?
We offer you a solution so that you could use valid and updated legislative regulations.
Would you like to get more information? Look at this page.
Latest update: 2026-05-17 (Number of items: 2 278 942)
© Copyright 2026 NORMSERVIS s.r.o.