We need your consent to use the individual data so that you can see information about your interests, among other things. Click "OK" to give your consent.
Heat Treatment of Low-Alloy Steel Parts Minimum Tensile Strength 220 ksi (1517 MPa) and Higher
Translate name
STANDARD published on 1.7.2021
Designation standards: SAE AMS2759/2K
Publication date standards: 1.7.2021
SKU: NS-1029413
Country: American technical standard
Category: Technical standards SAE
This specification, in conjunction with the general requirements for steel heat treatment covered in AMS2759, establishes the requirements for heat treatment of low-alloy steel parts to minimum ultimate tensile strengths of 220 ksi (1517 MPa) and higher. Parts are defined in AMS2759. The requirements for heat treatment of alloy Aermet100 are no longer part of this specification and can be found in AMS2759/3. Due to the limited hardenability of these materials, size limits have been added to this specification.
SUBFILE: Aerospace
TYPE OF DOCUMENT: Aerospace Material Specification
Do you want to be sure about the validity of used regulations?
We offer you a solution so that you could use valid and updated legislative regulations.
Would you like to get more information? Look at this page.
Latest update: 2024-03-25 (Number of items: 2 885 931)
© Copyright 2024 NORMSERVIS s.r.o.