Standard ASTM A875/A875M-23 1.10.2023 preview

ASTM A875/A875M-23

Standard Specification for Steel Sheet, Zinc-5 % Aluminum Alloy-Coated by the Hot-Dip Process

Translate name

STANDARD published on 1.10.2023


Language
Format
AvailabilityIN STOCK
Price69.00 USD excl. VAT
69.00 USD

The information about the standard:

Designation standards: ASTM A875/A875M-23
Publication date standards: 1.10.2023
SKU: NS-1157276
The number of pages: 12
Approximate weight : 36 g (0.08 lbs)
Country: American technical standard
Category: Technical standards ASTM

The category - similar standards:

Flat steel products and semi-products

Annotation of standard text ASTM A875/A875M-23 :

This specification covers steel sheet, in coils and cut lengths, metallic-coated by the hot-dip process, with zinc-aluminum alloy coating. The coating is produced as two types: zinc-aluminum-mischmetal alloy (Type I) and zinc-aluminum-magnesium alloy (Type II), and in two coating structures. Coated sheet is produced in several coating designations (coating weight [mass]). Material is classified in terms of the base metal and in terms of the coating. Base metal material classification is as follows: commercial steel (CS Types A, B, and C), forming steel (FS Types A and B), deep drawing steel (DDS), extra deep drawing steel (EDDS), structural steel (SS), high-strength low-alloy steel (HSLAS), and high-strength low-alloy steel with improved formability (HSLAS-F). Structural steel and high strength low alloy steel are available in several grades based on mechanical properties. Structural steel grade 50 [340] is available in three classes based on tensile strength. Heat analysis of the base metal for CS , FS, DDS, and EDDS shall conform to the chemical composition requirements in carbon, manganese, phosphorus, sulfur, aluminum, copper, nickel, chromium, molybdenum, vanadium, titanium, nitrogen, and boron and chemical composition in carbon, manganese, phosphorus, sulfur, copper, nickel, chromium, molybdenum, vanadium, titanium, nitrogen for SS, HSLAS, and HSLAS-F. Structural steel shall conform to the required yield strength, tensile strength, and elongation. Coating shall conform to the coating weight according to triple-spot test and single-spot test and shall be capable of bending without flaking.


Keywords:
coatings, metallic, steel sheet, zinc alloy coated, steel sheet, zinc coated, zinc alloys, zinc-coated steel, zinc-5 % aluminum-0.1 % magnesium alloy-coated steel, zinc-5 % aluminum alloy-coated steel, zinc-5 % aluminum-mischmetal alloy-coated steel,, ICS Number Code 77.140.50 (Flat steel products and semi-products)

We recommend:

Updating of laws

Do you want to be sure about the validity of used regulations?
We offer you a solution so that you could use valid and updated legislative regulations.
Would you like to get more information? Look at this page.




Cookies Cookies

We need your consent to use the individual data so that you can see information about your interests, among other things. Click "OK" to give your consent.

You can refuse consent here.

Here you can customize your cookie settings according to your preferences.

We need your consent to use the individual data so that you can see information about your interests, among other things.